I am about to order a big epoxy quantity from Raka. My shop is at 6,500 feet and the temp is usually 45-55 degrees F. My glassing experience is very limited. The temp will tend to be dropping during cure.
Suggestions on fast vs. medium vs. slow cure? Should I do a half & half order?
What about the "non-blushing"?
Suggestions on Thin vs. Medium vs. Thick epoxy resin?
(My first lamination I did last night was with some old West 205/105, after 12 hours still has quite a bit of curing to do).
Me: Do they take that as a mayfly or a caddis?
Willie: I don't know, I never asked them.